2328 Stainless Steels to SS 142328

2328 - Specification & Application

  • SS 142328 - Stainless steel - SS steel 2328

Stainless steel - SS steel 2328

Chemical composition(wt.%) of 2328 grade: to SS 142328

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.80
Mn - 1.20
P - 0.035
S - 0.020
Cr 24.00 26.00
Ni 6.00 8.00
Mo 3.50 5.00
N 0.24 0.32

2328 - Detail

Stainless steel - SS steel 2328

Mechanical properties of grade 2328 SS 142328

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
868 (≥) 156 (≥) 34 41 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 312

Physical properties of grade 2328 SS 142328

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
146 (≥) 783 (≥) 43 22 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 122
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
211 216 783

Equivalent Grade

Equivalent Products

We can customize the production of 2328 grade, contact us for the best solution.