2570 Stainless Steels to SS 142570

2570 - Specification & Application

  • SS 142570 - High-strength austenitic steel for use at elevated temperature

High-strength austenitic steel for use at elevated temperature

Chemical composition(wt.%) of 2570 grade: to SS 142570

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.025
S - 0.025
Cr 13.50 16.00
Ni 24.00 27.00
Mo 1.00 1.50
V 0.10 0.50
Ti 1.90 2.30
Al - 0.35
B 0.003 0.010

2570 - Detail

High-strength austenitic steel for use at elevated temperature

Mechanical properties of grade 2570 SS 142570

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
246 (≥) 542 (≥) 22 31 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 442

Physical properties of grade 2570 SS 142570

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
881 (≥) 515 (≥) 12 11 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 231
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
254 229 314

Equivalent Products

We can customize the production of 2570 grade, contact us for the best solution.