2HR401 Stainless Steels to BS 2HR 401 (1973)

2HR401 - Specification & Application

  • BS 2HR 401 (1973) - Specification for nickel-chromium-titanium-aluminium heat-resisting alloy cold worked and softened seamless tubes (nickel base, Cr 19.5, Ti 2.2, Al 1.4)
  • BS 3HR 401 (2011) - Specification for nickel-chromium-titanium-aluminium heat-resisting alloy seamless tubes (Nickel base, Cr 19.5, Ti 2.2, Al 1.4)

Specification for nickel-chromium-titanium-aluminium heat-resisting alloy seamless tubes (Nickel base, Cr 19.5, Ti 2.2, Al 1.4)

Chemical composition(wt.%) of 2HR401 grade: to BS 2HR 401 (1973)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.10
Si - 1.00
Mn - 1.00
P - -
S - 0.015
Cr 18.00 21.00
Ni - remaining
Mo - -
Co - 2.00
Ti 1.80 2.70
Fe - 1.50
Al 1.00 1.80
Cu - 0.20
B - 0.008
Bi - 0.0001
Pb - 0.002
Ag - 0.0005

2HR401 - Detail

Specification for nickel-chromium-titanium-aluminium heat-resisting alloy seamless tubes (Nickel base, Cr 19.5, Ti 2.2, Al 1.4)

Mechanical properties of grade 2HR401 BS 2HR 401 (1973)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
239 (≥) 173 (≥) 13 23 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 433

Physical properties of grade 2HR401 BS 2HR 401 (1973)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
843 (≥) 193 (≥) 21 33 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 323
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
743 729 368

Equivalent Grade

Equivalent Products

We can customize the production of 2HR401 grade, contact us for the best solution.