2S.137 Stainless Steels to BS 2S 137

2S.137 - Specification & Application

  • BS 2S 137 - Specification for high chromium-nickel corrosion-resisting steel bright bars (free machining) (880-1080 MPa: limiting ruling section 70 mm)

Specification for high chromium-nickel corrosion-resisting steel bright bars (free machining) (880-1080 MPa: limiting ruling section 70 mm)

Chemical composition(wt.%) of 2S.137 grade: to BS 2S 137

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.12 0.20
Si - 1.00
Mn - 1.50
P - 0.030
S 0.15 0.30
Cr 15.00 18.00
Ni 2.00 3.00
Mo - 0.60

2S.137 - Detail

Specification for high chromium-nickel corrosion-resisting steel bright bars (free machining) (880-1080 MPa: limiting ruling section 70 mm)

Mechanical properties of grade 2S.137 BS 2S 137

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
655 (≥) 971 (≥) 32 12 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade 2S.137 BS 2S 137

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
818 (≥) 962 (≥) 23 33 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 142
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
247 321 358

Equivalent Grade

Equivalent Products

We can customize the production of 2S.137 grade, contact us for the best solution.