3130 Stainless Steels

3130 - Specification & Application

3130

Chemical composition(wt.%) of 3130 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.25 0.32
Si 0.15 0.35
Mn 0.50 0.90
P - 0.040
S - 0.040
Cr 0.60 0.70
Ni 1.25 1.75

3130 - Detail

3315

Mechanical properties of grade 3130

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
757 (≥) 413 (≥) 41 21 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 343

Physical properties of grade 3130

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
263 (≥) 947 (≥) 33 41 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 221
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
142 493 468