331S40 Stainless Steels to BS 970-4

331S40 - Specification & Application

  • BS 970-4 - Specification for wrought steels for mechanical and allied engineering purposes. Valve steels

Specification for wrought steels for mechanical and allied engineering purposes. Valve steels

Chemical composition(wt.%) of 331S40 grade: to BS 970-4

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.35 0.50
Si 1.00 2.00
Mn 0.50 1.00
P - 0.040
S - 0.030
Cr 12.00 15.00
Ni 12.00 15.00
Mo - -
W 2.00 3.00

331S40 - Detail

Specification for wrought steels for mechanical and allied engineering purposes. Valve steels

Mechanical properties of grade 331S40 BS 970-4

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
546 (≥) 365 (≥) 12 14 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 411

Physical properties of grade 331S40 BS 970-4

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
392 (≥) 241 (≥) 13 23 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 243
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
763 891 886

Equivalent Grade

Equivalent Products

We can customize the production of 331S40 grade, contact us for the best solution.
sales@specificsteel.com