40CrMo5-6 Stainless Steels to ISO/TR 4956

40CrMo5-6 - Specification & Application

  • ISO/TR 4956 - Wrought steels for use at elevated temperatures in engines

Wrought steels for use at elevated temperatures in engines

Chemical composition(wt.%) of 40CrMo5-6 grade: to ISO/TR 4956

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.35 0.45
Si 0.15 0.40
Mn 0.40 0.70
P - 0.035
S - 0.035
Cr 1.00 1.50
Mo 0.50 0.80
Ni - -

40CrMo5-6 - Detail

Wrought steels for use at elevated temperatures in engines

Mechanical properties of grade 40CrMo5-6 ISO/TR 4956

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
779 (≥) 829 (≥) 12 23 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 421

Physical properties of grade 40CrMo5-6 ISO/TR 4956

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
154 (≥) 381 (≥) 11 41 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 421
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
732 528 299

Equivalent Grade

Equivalent Products

We can customize the production of 40CrMo5-6 grade, contact us for the best solution.