410S21 Stainless Steels to BS 1449-2

410S21 - Specification & Application

  • BS 1449-2 - Steel plate, sheet and strip. Specification for stainless and heat-resisting steel plate, sheet and strip
  • BS 1503 - Specification for steel forgings for pressure purposes
  • BS 1554 - Specification for stainless and heat-resisting steel round wire
  • BS 6258 - Specification for hollow steel bars for machining
  • BS 970-1 - Specification for wrought steels for mechanical and allied engineering purposes. General inspection and testing procedures and specific requirements for carbon, carbon manganese, alloy and stainless steels
  • BS 970-3 - Specification for wrought steels for mechanical and allied engineering purposes. Bright bars for general engineering purposes

Specification for wrought steels for mechanical and allied engineering purposes. Bright bars for general engineering purposes

Chemical composition(wt.%) of 410S21 grade: to BS 1449-2

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.09 0.15
Si - 1.00
Mn - 1.00
P - 0.04
S - 0.03
Cr 11.50 13.50
Mo - -
Ni - 1.00

410S21 - Detail

Specification for wrought steels for mechanical and allied engineering purposes. Bright bars for general engineering purposes

Mechanical properties of grade 410S21 BS 1449-2

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
838 (≥) 116 (≥) 22 21 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 414

Physical properties of grade 410S21 BS 1449-2

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
954 (≥) 682 (≥) 23 41 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 424
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
275 656 119

Equivalent Products

We can customize the production of 410S21 grade, contact us for the best solution.
sales@specificsteel.com