420J2CPS Stainless Steels

420J2CPS - Specification & Application

CNS standard spring cold rolled stainless steel strip

Chemical composition(wt.%) of 420J2CPS grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.26 0.40
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.030
Cr 12.00 14.00
Ni - 0.60

420J2CPS - Detail

CNS standard spring cold rolled stainless steel strip

Mechanical properties of grade 420J2CPS

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
792 (≥) 994 (≥) 42 44 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 434

Physical properties of grade 420J2CPS

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
978 (≥) 198 (≥) 43 43 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 143
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
837 639 961

Equivalent Grade

Equivalent Products

We can customize the production of 420J2CPS grade, contact us for the best solution.
sales@specificsteel.com