420S29 Stainless Steels to BS 1503

420S29 - Specification & Application

  • BS 1503 - Specification for steel forgings for pressure purposes
  • BS 1554 - Specification for stainless and heat-resisting steel round wire
  • BS 5770-4 - Steel strip intended for the manufacture of springs. Specification for martensitic and austenitic stainless steel
  • BS 970-1 - Specification for wrought steels for mechanical and allied engineering purposes. General inspection and testing procedures and specific requirements for carbon, carbon manganese, alloy and stainless steels
  • BS 970-3 - Specification for wrought steels for mechanical and allied engineering purposes. Bright bars for general engineering purposes

Specification for wrought steels for mechanical and allied engineering purposes. Bright bars for general engineering purposes

Chemical composition(wt.%) of 420S29 grade: to BS 1503

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.14 0.20
Si - 1.00
Mn - 1.00
P - 0.04
S - 0.03
Cr 11.50 13.50
Mo - -
Ni - 1.00

420S29 - Detail

Specification for wrought steels for mechanical and allied engineering purposes. Bright bars for general engineering purposes

Mechanical properties of grade 420S29 BS 1503

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
774 (≥) 263 (≥) 41 21 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 342

Physical properties of grade 420S29 BS 1503

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
592 (≥) 768 (≥) 34 22 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 441
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
892 516 494

Equivalent Grade

Equivalent Products

We can customize the production of 420S29 grade, contact us for the best solution.