615 Stainless Steels to A 565/A 565M (2010)

615 - Specification & Application

  • A 565/A 565M (2010) - Martensitic Stainless Steel Bars for High-Temperature Service

Martensitic Stainless Steel Bars for High-Temperature Service

Chemical composition(wt.%) of 615 grade: to A 565/A 565M (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.15 0.20
Si - 0.50
Mn - 0.50
P - 0.04
S - 0.03
Cr 12.0 14.0
Ni 1.80 2.20
Mo - 0.50
W 2.50 3.50

615 - Detail

Martensitic Stainless Steel Bars for High-Temperature Service

Mechanical properties of grade 615 A 565/A 565M (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
834 (≥) 648 (≥) 43 43 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 333

Physical properties of grade 615 A 565/A 565M (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
167 (≥) 347 (≥) 44 43 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 232
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
948 225 954