Standard Specification for Alloy-Steel and Stainless Steel Bolting for High Temperature or High Pressure Service and Other Special Purpose Applications
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.13 | ||
Si | - | - | ||
Mn | - | - | ||
Ni | - | - | ||
Cr | - | 5.70 | ||
Al | - | 6.30 | ||
Cu | - | - | ||
Ti | - | - | ||
Fe | - | - | ||
Mo | - | 2.00 | ||
Co | - | - | ||
Ta | - | 3.00 | ||
Zr | - | 0.60 | ||
W | - | 11.00 |
Standard Specification for Alloy-Steel and Stainless Steel Bolting for High Temperature or High Pressure Service and Other Special Purpose Applications
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
322 (≥) | 315 (≥) | 44 | 22 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 323 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
225 (≥) | 234 (≥) | 13 | 23 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 243 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
548 | 257 | 184 |
We can customize the production of A 193 B8M2 Class 2B grade, contact us for the best solution.