A 213 N08904 Stainless Steels to A 213/A 213M (2013)

A 213 N08904 - Specification & Application

  • A 213/A 213M (2013) - Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Chemical composition(wt.%) of A 213 N08904 grade: to A 213/A 213M (2013)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.02
Mn - 2.00
Si - 1.00
P - 0.045
S - 0.035
Cr 19.00 23.00
Ni 23.00 28.00
Mo 4.00 5.00
Cu 1.00 2.00

A 213 N08904 - Detail

Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Mechanical properties of grade A 213 N08904 A 213/A 213M (2013)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
172 (≥) 428 (≥) 34 14 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 334

Physical properties of grade A 213 N08904 A 213/A 213M (2013)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
383 (≥) 162 (≥) 14 24 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
826 276 199