A 268 S44800 Stainless Steels to A 268/A 268M (2010)

A 268 S44800 - Specification & Application

  • A 268/A 268M (2010) - Seamless and Welded Ferritic and Martensitic Stainless Steel Tubing for General Service

Seamless and Welded Ferritic and Martensitic Stainless Steel Tubing for General Service

Chemical composition(wt.%) of A 268 S44800 grade: to A 268/A 268M (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Mn - 0.30
Si - 0.20
P - 0.025
S - 0.02
Cr 28.00 30.00
Ni 2.00 2.50
Mo 3.50 4.20
N - 0.02
Cu - 0.15

A 268 S44800 - Detail

Seamless and Welded Ferritic and Martensitic Stainless Steel Tubing for General Service

Mechanical properties of grade A 268 S44800 A 268/A 268M (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
432 (≥) 484 (≥) 41 32 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 323

Physical properties of grade A 268 S44800 A 268/A 268M (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
956 (≥) 354 (≥) 31 13 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 324
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
592 939 112

Equivalent Products

We can customize the production of A 268 S44800 grade, contact us for the best solution.