A 276 S24100 Stainless Steels to A 276 (2013)

A 276 S24100 - Specification & Application

  • A 276 (2013) - Stainless Steel Bars and Shapes

Stainless Steel Bars and Shapes

Chemical composition(wt.%) of A 276 S24100 grade: to A 276 (2013)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Mn 11.00 14.00
Si - 1.00
P - 0.06
S - 0.03
Cr 16.50 19.50
Ni 0.50 2.50
Mo - -
N 0.20 0.45

A 276 S24100 - Detail

Stainless Steel Bars and Shapes

Mechanical properties of grade A 276 S24100 A 276 (2013)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
944 (≥) 413 (≥) 31 43 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 241

Physical properties of grade A 276 S24100 A 276 (2013)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
988 (≥) 826 (≥) 43 42 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 131
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
331 595 156
We can customize the production of A 276 S24100 grade, contact us for the best solution.