A 312 S30815 Stainless Steels to A 312/A 312M (2013)

A 312 S30815 - Specification & Application

  • A 312/A 312M (2013) - Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes

Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes

Chemical composition(wt.%) of A 312 S30815 grade: to A 312/A 312M (2013)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.05 0.10
Mn - 0.80
Si 1.40 2.00
P - 0.04
S - 0.03
Cr 20.00 22.00
Ni 10.00 12.00
Mo - -
Al - 1.00
Ce 0.03 0.08

A 312 S30815 - Detail

Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes

Mechanical properties of grade A 312 S30815 A 312/A 312M (2013)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
274 (≥) 444 (≥) 13 32 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 214

Physical properties of grade A 312 S30815 A 312/A 312M (2013)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
383 (≥) 287 (≥) 23 23 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 314
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
397 557 966

Equivalent Products

We can customize the production of A 312 S30815 grade, contact us for the best solution.