A 358 N08800 Stainless Steels to A 358/A 358M (2012)

A 358 N08800 - Specification & Application

  • A 358/A 358M (2012) - Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Chemical composition(wt.%) of A 358 N08800 grade: to A 358/A 358M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Mn - 1.50
Si - 1.00
P - 0.045
S - 0.015
Cr 19.00 23.00
Ni 30.00 35.00
Mo - -
Ti 0.15 0.60
Al 0.15 0.60

A 358 N08800 - Detail

Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Mechanical properties of grade A 358 N08800 A 358/A 358M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
215 (≥) 419 (≥) 44 23 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 111

Physical properties of grade A 358 N08800 A 358/A 358M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
465 (≥) 214 (≥) 42 14 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 334
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
355 369 358