A 358 S30415 Stainless Steels to A 358/A 358M (2012)

A 358 S30415 - Specification & Application

  • A 358/A 358M (2012) - Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Chemical composition(wt.%) of A 358 S30415 grade: to A 358/A 358M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Mn - 0.60
Si - 1.30
P - -
S - -
Cr - 18.5
Ni - 9.50
Mo - -
N - 0.15
Ce - 0.04

A 358 S30415 - Detail

Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Mechanical properties of grade A 358 S30415 A 358/A 358M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
538 (≥) 837 (≥) 11 44 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 331

Physical properties of grade A 358 S30415 A 358/A 358M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
832 (≥) 189 (≥) 44 41 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 313
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
761 242 175

Equivalent Products

We can customize the production of A 358 S30415 grade, contact us for the best solution.