A 358 S31040 Stainless Steels to A 358/A 358M (2012)

A 358 S31040 - Specification & Application

  • A 358/A 358M (2012) - Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Chemical composition(wt.%) of A 358 S31040 grade: to A 358/A 358M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Mn - 2.00
Si - 1.50
P - 0.045
S - 0.03
Cr 24.00 26.00
Ni 19.00 22.00
Mo - -
Nb+Ta 10×C% 1.10

A 358 S31040 - Detail

Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Mechanical properties of grade A 358 S31040 A 358/A 358M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
913 (≥) 419 (≥) 13 22 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 323

Physical properties of grade A 358 S31040 A 358/A 358M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
967 (≥) 858 (≥) 22 32 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 443
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
258 375 217

Equivalent Products

We can customize the production of A 358 S31040 grade, contact us for the best solution.