A 409 S30815 Stainless Steels to A 409/A 409M (2009)

A 409 S30815 - Specification & Application

  • A 409/A 409M (2009) - Welded Large Diameter Austenitic Steel Pipe for Corrosive or High-Temperature Service

Welded Large Diameter Austenitic Steel Pipe for Corrosive or High-Temperature Service

Chemical composition(wt.%) of A 409 S30815 grade: to A 409/A 409M (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.05 0.10
Mn - 0.80
Si 1.40 2.00
P - 0.04
S - 0.03
Cr 20.00 22.00
Ni 10.00 12.00
Mo - -
Al - 1.00
Ce 0.03 0.08

A 409 S30815 - Detail

Welded Large Diameter Austenitic Steel Pipe for Corrosive or High-Temperature Service

Mechanical properties of grade A 409 S30815 A 409/A 409M (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
645 (≥) 643 (≥) 43 11 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 221

Physical properties of grade A 409 S30815 A 409/A 409M (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
241 (≥) 757 (≥) 31 11 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 213
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
833 496 249