A 479 S31726 Stainless Steels to A 479/A 479M (2013)

A 479 S31726 - Specification & Application

  • A 479/A 479M (2013) - Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels

Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels

Chemical composition(wt.%) of A 479 S31726 grade: to A 479/A 479M (2013)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 2.00
Si - 0.75
P - 0.045
S - 0.03
Cr 17.00 20.00
Ni 13.50 17.50
Mo 4.00 5.00
N 0.10 0.20

A 479 S31726 - Detail

Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels

Mechanical properties of grade A 479 S31726 A 479/A 479M (2013)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
522 (≥) 518 (≥) 31 12 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 414

Physical properties of grade A 479 S31726 A 479/A 479M (2013)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
574 (≥) 732 (≥) 12 11 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 442
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
394 117 524

Equivalent Products

We can customize the production of A 479 S31726 grade, contact us for the best solution.