A 646 Grade Nit. 135 Stainless Steels to A 646/A 646M (2011)

A 646 Grade Nit. 135 - Specification & Application

  • A 646/A 646M (2011) - Premium Quality Alloy Steel Blooms and Billets for Aircraft and Aerospace Forgings

Premium Quality Alloy Steel Blooms and Billets for Aircraft and Aerospace Forgings

Chemical composition(wt.%) of A 646 Grade Nit. 135 grade: to A 646/A 646M (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.38 0.43
Si 0.20 0.40
Mn 0.50 0.70
Cr - -
Ni 0.30 0.40
Mo - -
Co - -
W 0.95 1.30
Al - -
Cu - -
Ti - -
Fe - -

A 646 Grade Nit. 135 - Detail

Premium Quality Alloy Steel Blooms and Billets for Aircraft and Aerospace Forgings

Mechanical properties of grade A 646 Grade Nit. 135 A 646/A 646M (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
338 (≥) 832 (≥) 22 34 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 223

Physical properties of grade A 646 Grade Nit. 135 A 646/A 646M (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
178 (≥) 911 (≥) 42 23 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 313
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
922 685 657