A 666 S31651 Stainless Steels to A 666 (2010)

A 666 S31651 - Specification & Application

  • A 666 (2010) - Annealed or Cold-Worked Austenitic Stainless Steel Sheet, Strip, Plate, and Flat Bar

Annealed or Cold-Worked Austenitic Stainless Steel Sheet, Strip, Plate, and Flat Bar

Chemical composition(wt.%) of A 666 S31651 grade: to A 666 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 16.0 18.0
Ni 10.0 14.0
Mo 2.00 3.00
N 0.10 0.16

A 666 S31651 - Detail

Annealed or Cold-Worked Austenitic Stainless Steel Sheet, Strip, Plate, and Flat Bar

Mechanical properties of grade A 666 S31651 A 666 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
517 (≥) 242 (≥) 41 12 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade A 666 S31651 A 666 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
216 (≥) 385 (≥) 13 12 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 443
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
469 955 564