A 688 N08800 Stainless Steels to A 688/A 688M (2012)

A 688 N08800 - Specification & Application

  • A 688/A 688M (2012) - Welded Austenitic Stainless Steel Feedwater Heater Tubes

Welded Austenitic Stainless Steel Feedwater Heater Tubes

Chemical composition(wt.%) of A 688 N08800 grade: to A 688/A 688M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Mn - 1.50
Si - 1.00
P - 0.045
S - 0.015
Cr 19.00 23.00
Ni 30.00 35.00
Mo - -
Ti 0.15 0.60
Al 0.15 0.60

A 688 N08800 - Detail

Welded Austenitic Stainless Steel Feedwater Heater Tubes

Mechanical properties of grade A 688 N08800 A 688/A 688M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
991 (≥) 285 (≥) 14 42 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 444

Physical properties of grade A 688 N08800 A 688/A 688M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
776 (≥) 714 (≥) 14 21 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
328 825 254

Equivalent Products

We can customize the production of A 688 N08800 grade, contact us for the best solution.
sales@specificsteel.com