A 693 S17400 Stainless Steels to A 693 (2006)

A 693 S17400 - Specification & Application

  • A 693 (2006) - Precipitation-Hardening Stainless and Heat-Resisting Steel Plate, Sheet, and Strip

Precipitation-Hardening Stainless and Heat-Resisting Steel Plate, Sheet, and Strip

Chemical composition(wt.%) of A 693 S17400 grade: to A 693 (2006)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.07
Mn - 1.00
Si - 1.00
P - 0.04
S - 0.03
Cr 15.00 17.50
Ni 3.00 5.00
Mo - -
Cu 3.00 5.00
Nb+Ta 0.15 0.45

A 693 S17400 - Detail

Precipitation-Hardening Stainless and Heat-Resisting Steel Plate, Sheet, and Strip

Mechanical properties of grade A 693 S17400 A 693 (2006)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
214 (≥) 842 (≥) 21 12 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 431

Physical properties of grade A 693 S17400 A 693 (2006)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
811 (≥) 492 (≥) 43 43 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 414
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
258 977 348