A 928 S32304 Stainless Steels to A 928/A 928M (2011)

A 928 S32304 - Specification & Application

  • A 928/A 928M (2011) - Ferritic/Austenitic (Duplex) Stainless Steel Pipe Electric Fusion Welded with Addition of Filler Metal

Ferritic/Austenitic (Duplex) Stainless Steel Pipe Electric Fusion Welded with Addition of Filler Metal

Chemical composition(wt.%) of A 928 S32304 grade: to A 928/A 928M (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 2.50
Si - 1.00
P - 0.04
S - 0.04
Cr 21.50 24.50
Ni 3.00 5.50
Mo 0.05 0.60
N 0.05 0.20
Cu 0.05 0.60

A 928 S32304 - Detail

Ferritic/Austenitic (Duplex) Stainless Steel Pipe Electric Fusion Welded with Addition of Filler Metal

Mechanical properties of grade A 928 S32304 A 928/A 928M (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
748 (≥) 375 (≥) 43 23 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 314

Physical properties of grade A 928 S32304 A 928/A 928M (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
277 (≥) 955 (≥) 21 22 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 424
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
442 831 612

Equivalent Products

We can customize the production of A 928 S32304 grade, contact us for the best solution.
sales@specificsteel.com