A 928 S32550 Stainless Steels to A 928/A 928M (2011)

A 928 S32550 - Specification & Application

  • A 928/A 928M (2011) - Ferritic/Austenitic (Duplex) Stainless Steel Pipe Electric Fusion Welded with Addition of Filler Metal

Ferritic/Austenitic (Duplex) Stainless Steel Pipe Electric Fusion Welded with Addition of Filler Metal

Chemical composition(wt.%) of A 928 S32550 grade: to A 928/A 928M (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.04
Mn - 1.50
Si - 1.00
P - 0.04
S - 0.03
Cr 24.00 27.00
Ni 4.50 6.50
Mo 2.00 4.00
N 0.10 0.25
Cu 1.50 2.50

A 928 S32550 - Detail

Ferritic/Austenitic (Duplex) Stainless Steel Pipe Electric Fusion Welded with Addition of Filler Metal

Mechanical properties of grade A 928 S32550 A 928/A 928M (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
679 (≥) 136 (≥) 44 42 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 144

Physical properties of grade A 928 S32550 A 928/A 928M (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
553 (≥) 715 (≥) 22 42 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 143
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
818 815 196