A 959 S30815 Stainless Steels to A 959 (2011)

A 959 S30815 - Specification & Application

  • A 959 (2011) - Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels

Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels

Chemical composition(wt.%) of A 959 S30815 grade: to A 959 (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.05 0.10
Si 1.40 2.00
Mn - 0.80
P - 0.04
S - 0.03
Cr 20.0 22.0
Ni 10.00 12.0
N 0.14 0.20
Ce 0.03 0.08

A 959 S30815 - Detail

Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels

Mechanical properties of grade A 959 S30815 A 959 (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
282 (≥) 279 (≥) 44 43 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 212

Physical properties of grade A 959 S30815 A 959 (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
348 (≥) 162 (≥) 42 34 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 342
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
243 323 473