A 988 N08367 Stainless Steels to A 988/A 988M (2011)

A 988 N08367 - Specification & Application

  • A 988/A 988M (2011) - Hot Isostatically-Pressed Stainless Steel Flanges, Fittings, Valves, and Parts for High Temperature Service

Hot Isostatically-Pressed Stainless Steel Flanges, Fittings, Valves, and Parts for High Temperature Service

Chemical composition(wt.%) of A 988 N08367 grade: to A 988/A 988M (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 2.00
Si - 1.00
P - 0.04
S - 0.03
Cr 20.00 22.00
Ni 23.50 25.50
Mo 6.00 7.00
N 0.18 0.25

A 988 N08367 - Detail

Hot Isostatically-Pressed Stainless Steel Flanges, Fittings, Valves, and Parts for High Temperature Service

Mechanical properties of grade A 988 N08367 A 988/A 988M (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
845 (≥) 475 (≥) 14 42 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 444

Physical properties of grade A 988 N08367 A 988/A 988M (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
391 (≥) 249 (≥) 31 41 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 111
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
217 987 517
We can customize the production of A 988 N08367 grade, contact us for the best solution.