B 462 N08024 Stainless Steels to B 462 (2010)

B 462 N08024 - Specification & Application

  • B 462 (2010) - Standard Specification for Forged or Rolled UNS N06030, UNS N06022, UNS N06035, UNS N06200, UNS N06059, UNS N10362, UNS N06686, UNS N08020, UNS N08024, UNS N08026, UNS N08367, UNS N10276, UNS N10665, UNS N10675, UNS N10629, UNS N08031, UNS N06045

Standard Specification for Forged or Rolled UNS N06030, UNS N06022, UNS N06035, UNS N06200, UNS N06059, UNS N10362, UNS N06686, UNS N08020, UNS N08024, UNS N08026, UNS N08367, UNS N10276, UNS N10665, UNS N10675, UNS N10629, UNS N08031, UNS N06045

Chemical composition(wt.%) of B 462 N08024 grade: to B 462 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 1.00
Si - 0.50
P - 0.035
S - 0.035
Cr 22.50 25.00
Ni 35.00 40.00
Mo 3.50 5.00
Cu 0.50 1.50
Nb 0.15 0.35

B 462 N08024 - Detail

Standard Specification for Forged or Rolled UNS N06030, UNS N06022, UNS N06035, UNS N06200, UNS N06059, UNS N10362, UNS N06686, UNS N08020, UNS N08024, UNS N08026, UNS N08367, UNS N10276, UNS N10665, UNS N10675, UNS N10629, UNS N08031, UNS N06045

Mechanical properties of grade B 462 N08024 B 462 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
514 (≥) 258 (≥) 22 33 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 242

Physical properties of grade B 462 N08024 B 462 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
786 (≥) 862 (≥) 11 33 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 212
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
283 779 353

Equivalent Products

We can customize the production of B 462 N08024 grade, contact us for the best solution.