B 475 N08026 Stainless Steels to B 475 (2007)

B 475 N08026 - Specification & Application

  • B 475 (2007) - UNS N08020, UNS N08024, and UNS N08026 Nickel Alloy Round Weaving Wire

UNS N08020, UNS N08024, and UNS N08026 Nickel Alloy Round Weaving Wire

Chemical composition(wt.%) of B 475 N08026 grade: to B 475 (2007)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 1.00
Si - 0.50
P - 0.03
S - 0.03
Cr 22.00 26.00
Ni 33.00 37.20
Mo 5.00 6.70
Cu 2.00 4.00

B 475 N08026 - Detail

UNS N08020, UNS N08024, and UNS N08026 Nickel Alloy Round Weaving Wire

Mechanical properties of grade B 475 N08026 B 475 (2007)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
523 (≥) 481 (≥) 43 22 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 332

Physical properties of grade B 475 N08026 B 475 (2007)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
291 (≥) 346 (≥) 14 31 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 314
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
733 899 621

Equivalent Products

We can customize the production of B 475 N08026 grade, contact us for the best solution.