B 536 N08330 Stainless Steels to B 536 (2007)

B 536 N08330 - Specification & Application

  • B 536 (2007) - Nickel-Iron-Chromium-Silicon Alloys (UNS N08330 and N08332) Plate, Sheet, and Strip

Nickel-Iron-Chromium-Silicon Alloys (UNS N08330 and N08332) Plate, Sheet, and Strip

Chemical composition(wt.%) of B 536 N08330 grade: to B 536 (2007)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Mn - 2.00
Si - 1.50
P - 0.045
S - 0.04
Cr 14.00 17.00
Ni 33.00 37.00

B 536 N08330 - Detail

Nickel-Iron-Chromium-Silicon Alloys (UNS N08330 and N08332) Plate, Sheet, and Strip

Mechanical properties of grade B 536 N08330 B 536 (2007)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
761 (≥) 498 (≥) 42 14 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 232

Physical properties of grade B 536 N08330 B 536 (2007)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
535 (≥) 615 (≥) 14 41 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 424
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
331 612 287

Equivalent Products

We can customize the production of B 536 N08330 grade, contact us for the best solution.