EV5 Stainless Steels

EV5 - Specification & Application

Steel for exhaust valves

Chemical composition(wt.%) of EV5 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.30 0.45
Si 2.75 3.25
Mn 0.80 1.30
P - 0.040
S - 0.030
Cr 18.0 20.0
Ni 7.50 8.50

EV5 - Detail

Steel for exhaust valves

Mechanical properties of grade EV5

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
411 (≥) 142 (≥) 24 34 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 433

Physical properties of grade EV5

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
538 (≥) 989 (≥) 41 23 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
119 324 169

Equivalent Products

We can customize the production of EV5 grade, contact us for the best solution.