EX 45 Stainless Steels to SAE J 1249 (2000)

EX 45 - Specification & Application

  • SAE J 1249 (2000) - Former SAE standard and former SAE Ex-steels

Former SAE standard and former SAE Ex-steels

Chemical composition(wt.%) of EX 45 grade: to SAE J 1249 (2000)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.25
Si - -
Mn - -
Cr - 25.50
Ni - 10.50
Mo - -
Co - 55.00
W - 7.00
Al - -
Cu - -
Ti - -
Fe - 2.00
B - 0.01

EX 45 - Detail

Former SAE standard and former SAE Ex-steels

Mechanical properties of grade EX 45 SAE J 1249 (2000)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
245 (≥) 221 (≥) 41 43 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 442

Physical properties of grade EX 45 SAE J 1249 (2000)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
532 (≥) 551 (≥) 42 13 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 122
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
169 427 696

Equivalent Grade

Equivalent Products

We can customize the production of EX 45 grade, contact us for the best solution.