F 837 Class A1-50 S38400 Stainless Steels to F 837M (2002)

F 837 Class A1-50 S38400 - Specification & Application

  • F 837M (2002) - Standard Specification for Stainless Steel Socket Head Cap Screws (Metric)

Standard Specification for Stainless Steel Socket Head Cap Screws (Metric)

Chemical composition(wt.%) of F 837 Class A1-50 S38400 grade: to F 837M (2002)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Mn - 2.00
Si - 1.00
P - 0.03
S - 0.03
Cr 15.00 17.00
Ni 17.00 19.00

F 837 Class A1-50 S38400 - Detail

Standard Specification for Stainless Steel Socket Head Cap Screws (Metric)

Mechanical properties of grade F 837 Class A1-50 S38400 F 837M (2002)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
692 (≥) 497 (≥) 42 32 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 431

Physical properties of grade F 837 Class A1-50 S38400 F 837M (2002)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
743 (≥) 439 (≥) 34 43 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 413
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
156 899 914