F738 Class C4-50 S41623 Stainless Steels to F 738M (2002)

F738 Class C4-50 S41623 - Specification & Application

  • F 738M (2002) - Standard Specification for Stainless Steel Metric Bolts, Screws, and Studs

Standard Specification for Stainless Steel Metric Bolts, Screws, and Studs

Chemical composition(wt.%) of F738 Class C4-50 S41623 grade: to F 738M (2002)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.15 -
Mn - 1.25
Si - 1.00
P - 0.06
S - 0.06
Cr 12.00 14.00
Ni - -
Mo - 0.60
Se 0.15 -

F738 Class C4-50 S41623 - Detail

Standard Specification for Stainless Steel Metric Bolts, Screws, and Studs

Mechanical properties of grade F738 Class C4-50 S41623 F 738M (2002)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
153 (≥) 951 (≥) 13 13 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 224

Physical properties of grade F738 Class C4-50 S41623 F 738M (2002)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
917 (≥) 159 (≥) 31 13 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 244
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
897 464 421