GMR-235D Stainless Steels to SAE J 467 (1968)

GMR-235D - Specification & Application

  • SAE J 467 (1968) - Special Purpose Alloys ("Superalloys")

Special Purpose Alloys ("Superalloys")

Chemical composition(wt.%) of GMR-235D grade: to SAE J 467 (1968)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 0.30
Mn - 0.13
P - -
S - -
Ni - remaining
Cr - 15.50
Al - 3.00
Cu - -
Ti - 2.00
Fe - 10.00
Mo - 5.25
Co - -
B - 0.06

GMR-235D - Detail

Special Purpose Alloys ("Superalloys")

Mechanical properties of grade GMR-235D SAE J 467 (1968)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
949 (≥) 318 (≥) 42 41 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 111

Physical properties of grade GMR-235D SAE J 467 (1968)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
341 (≥) 446 (≥) 21 11 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 314
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
674 759 987

Equivalent Grade

Equivalent Products

We can customize the production of GMR-235D grade, contact us for the best solution.