H86450 Stainless Steels

H86450 - Specification & Application

Steel for intake valves

Chemical composition(wt.%) of H86450 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.42 0.49
Si 0.15 0.30
Mn 0.70 1.05
P - 0.035
S - 0.04
Cr 0.35 0.65
Ni 0.35 0.75
Mo 0.15 0.25

H86450 - Detail

Steel for intake valves

Mechanical properties of grade H86450

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
114 (≥) 126 (≥) 14 12 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 312

Physical properties of grade H86450

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
368 (≥) 354 (≥) 44 41 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 133
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
688 796 899