HNV7(71360) Stainless Steels

HNV7(71360) - Specification & Application

Steel for intake valves

Chemical composition(wt.%) of HNV7(71360) grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.55 -
Si 0.20 -
Mn 0.20 -
P -
S -
Cr 3.50 -
W 14.0 -

HNV7(71360) - Detail

Steel for intake valves

Mechanical properties of grade HNV7(71360)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
575 (≥) 458 (≥) 43 11 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 133

Physical properties of grade HNV7(71360)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
226 (≥) 873 (≥) 33 31 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 414
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
888 452 145
We can customize the production of HNV7(71360) grade, contact us for the best solution.