HR10 Stainless Steels to BS HR 10 (1972)

HR10 - Specification & Application

  • BS HR 10 (1972) - Specification for nickel-cobalt-chromium-molybdenum-titanium-aluminium heat-resisting alloy billets, bars, forgings and parts (nickel base, Co 20, Cr 20, Mo 5.9, Ti 2.1, Al 0.5)
  • BS 2HR 10 (2010) - Specification for nickel-cobalt-chromium-molybdenum-titanium-aluminium heat-resisting alloy billets, bars, forgings and parts (nickel base, Co 20, Cr 20, Mo 5.9, Ti 2.1, Al 0.5)

Specification for nickel-cobalt-chromium-molybdenum-titanium-aluminium heat-resisting alloy billets, bars, forgings and parts (nickel base, Co 20, Cr 20, Mo 5.9, Ti 2.1, Al 0.5)

Chemical composition(wt.%) of HR10 grade: to BS HR 10 (1972)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.08
Si 0.40 -
Mn 0.60 -
P - -
S - 0.007
Cr 19.00 21.00
Ni - remaining
Mo 5.60 6.10
Co 19.00 21.00
Ti 1.90 2.40
Fe - 0.70
Al 0.30 0.60
Al+Ti 2.40 2.80

HR10 - Detail

Specification for nickel-cobalt-chromium-molybdenum-titanium-aluminium heat-resisting alloy billets, bars, forgings and parts (nickel base, Co 20, Cr 20, Mo 5.9, Ti 2.1, Al 0.5)

Mechanical properties of grade HR10 BS HR 10 (1972)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
119 (≥) 295 (≥) 31 22 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 342

Physical properties of grade HR10 BS HR 10 (1972)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
335 (≥) 971 (≥) 12 12 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 111
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
937 937 595

Equivalent Grade

Equivalent Products

We can customize the production of HR10 grade, contact us for the best solution.