HR3 Stainless Steels to BS HR 3

HR3 - Specification & Application

  • BS HR 3 - Specification for nickel-cobalt-chromium-molybdenum-aluminium-titanium heat-resisting alloy billets, bars, forgings and parts (nickel base, Co 20, Cr 14.8, Mo 5, Al 4.7, Ti 1.2)
  • BS 2HR 3 (2010) - Specification for nickel-cobalt-chromium-molybdenum-aluminium-titanium heat-resisting alloy billets, bars, forgings and parts (nickel base, Co 20, Cr 14.8, Mo 5, Al 4.8, Ti 1.2)

Specification for nickel-cobalt-chromium-molybdenum-aluminium-titanium heat-resisting alloy billets, bars, forgings and parts (nickel base, Co 20, Cr 14.8, Mo 5, Al 4.8, Ti 1.2)

Chemical composition(wt.%) of HR3 grade: to BS HR 3

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.12 0.17
Si - 1.00
Mn - 1.00
P - -
S - 0.015
Cr 14.00 15.70
Ni - remaining
Mo 4.50 5.50
Co 18.00 22.00
Ti 0.90 1.50
Fe - 1.00
Al 4.50 4.90
Cu - 0.20
B 0.0030 0.0100
Bi - 0.0001
Pb - 0.0015
Ag - 0.0005
Zr - 0.15

HR3 - Detail

Specification for nickel-cobalt-chromium-molybdenum-aluminium-titanium heat-resisting alloy billets, bars, forgings and parts (nickel base, Co 20, Cr 14.8, Mo 5, Al 4.8, Ti 1.2)

Mechanical properties of grade HR3 BS HR 3

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
193 (≥) 778 (≥) 22 41 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 334

Physical properties of grade HR3 BS HR 3

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
891 (≥) 771 (≥) 24 21 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 212
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
482 367 875

Equivalent Grade

Equivalent Products

We can customize the production of HR3 grade, contact us for the best solution.