Specification for heat-resisting alloy billets, bars, forgings and parts (Ni 25.5, Cr 14.7, Ti 2, Mn 1.5, Mo 1.2, Si 0.7, V 0.3, Fe remainder)
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.08 | ||
Si | - | 1.00 | ||
Mn | - | 2.00 | ||
P | - | 0.020 | ||
S | - | 0.015 | ||
Cr | 13.50 | 16.00 | ||
Ni | 24.00 | 27.00 | ||
Mo | 1.00 | 1.50 | ||
Co | - | - | ||
Ti | 1.90 | 2.30 | ||
Fe | - | remaining | ||
Al | - | 0.35 | ||
V | 0.10 | 0.50 | ||
B | 0.0030 | 0.0100 | ||
Pb | - | 0.005 |
Specification for heat-resisting alloy billets, bars, forgings and parts (Ni 25.5, Cr 14.7, Ti 2, Mn 1.5, Mo 1.2, Si 0.7, V 0.3, Fe remainder)
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
278 (≥) | 721 (≥) | 23 | 21 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 131 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
673 (≥) | 355 (≥) | 34 | 41 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 341 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
254 | 218 | 442 |
We can customize the production of HR51 grade, contact us for the best solution.