HR52 Stainless Steels to BS 2HR 52 (2010)

HR52 - Specification & Application

  • BS 2HR 52 (2010) - Specification for heat-resisting steel billets, bars, forgings and parts (Ni 25.5, Cr 14.7, Ti 1.8, Mn 1.5, Mo 1.2, V 0.3)
  • BS HR 52 - Specification for heat-resisting alloy billets, bars, forgings and parts (Ni 25.5, Cr 14.7, Ti 1.8, Mn 1.5, Mo 1.2, V 0.3, Fe remainder)

Specification for heat-resisting alloy billets, bars, forgings and parts (Ni 25.5, Cr 14.7, Ti 1.8, Mn 1.5, Mo 1.2, V 0.3, Fe remainder)

Chemical composition(wt.%) of HR52 grade: to BS 2HR 52 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Si - 0.50
Mn - 2.00
P - 0.020
S - 0.015
Cr 13.50 16.00
Ni 24.00 27.00
Mo 1.00 1.50
Co - -
Ti 1.70 2.00
Fe - remaining
Al - 0.35
V 0.10 0.50
B 0.0030 0.0100
Pb - 0.005

HR52 - Detail

Specification for heat-resisting alloy billets, bars, forgings and parts (Ni 25.5, Cr 14.7, Ti 1.8, Mn 1.5, Mo 1.2, V 0.3, Fe remainder)

Mechanical properties of grade HR52 BS 2HR 52 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
518 (≥) 689 (≥) 21 32 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 334

Physical properties of grade HR52 BS 2HR 52 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
825 (≥) 379 (≥) 34 11 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 444
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
154 784 854