HR53 Stainless Steels to BS 2HR 53 (2010)

HR53 - Specification & Application

  • BS 2HR 53 (2010) - Specification for nickel-iron-chromium-molybdenum-titanium heat-resisting alloy billets, bars, forgings and parts (Ni/Co 42.5, Cr 12.5, Mo 5.8, Ti 3.0, Fe remainder)
  • BS HR 53 - Specification for nickel-iron-chromium-molybdenum-titanium heat-resisting alloy billets, bars, forgings and parts (Ni/Co 42.5, Cr 12.5, Mo 5.8, Ti 3.0, Fe remainder)

Specification for nickel-iron-chromium-molybdenum-titanium heat-resisting alloy billets, bars, forgings and parts (Ni/Co 42.5, Cr 12.5, Mo 5.8, Ti 3.0, Fe remainder)

Chemical composition(wt.%) of HR53 grade: to BS 2HR 53 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.02 0.06
Si - 0.40
Mn - 0.50
P - 0.020
S - 0.020
Cr 11.00 14.00
Ni 40.00 45.00
Mo 5.00 6.50
Co - 1.00
Ti 2.80 3.10
Fe - remaining
Al - 0.30
Cu - 0.20
B 0.010 0.020
Pb - 0.0010
Bi - 0.0001
Ag - 0.0005

HR53 - Detail

Specification for nickel-iron-chromium-molybdenum-titanium heat-resisting alloy billets, bars, forgings and parts (Ni/Co 42.5, Cr 12.5, Mo 5.8, Ti 3.0, Fe remainder)

Mechanical properties of grade HR53 BS 2HR 53 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
491 (≥) 463 (≥) 42 33 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 443

Physical properties of grade HR53 BS 2HR 53 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
844 (≥) 626 (≥) 42 14 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 112
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
137 828 183

Equivalent Grade

Equivalent Products

We can customize the production of HR53 grade, contact us for the best solution.