HR55 Stainless Steels to BS 2HR 55 (2010)

HR55 - Specification & Application

  • BS 2HR 55 (2010) - Specification for nickel-iron-chromium-molybdenum-aluminium-titanium heat-resisting alloy billets, bars, forgings and parts (Ni/Co 43.5, Cr 16.5, Mo 3.3, Al 1.2, Ti 1.2, Fe remainder)
  • BS HR 55 - Specification for nickel-iron-chromium-molybdenum-aluminium-titanium heat-resisting alloy billets, bars, forgings and parts (Ni/Co 43.5, Cr 16.5, Mo 3.3, Al 1.2, Ti 1.2, Fe remainder)

Specification for nickel-iron-chromium-molybdenum-aluminium-titanium heat-resisting alloy billets, bars, forgings and parts (Ni/Co 43.5, Cr 16.5, Mo 3.3, Al 1.2, Ti 1.2, Fe remainder)

Chemical composition(wt.%) of HR55 grade: to BS 2HR 55 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.08
Si - 0.50
Mn - 0.20
P - -
S - 0.015
Cr 15.50 17.50
Ni 42.00 45.00
Mo 2.80 3.80
Co - 2.00
Ti 1.10 1.30
Fe - remaining
Al 1.10 1.30
Cu - 0.50
B - 0.005
Pb - 0.0015
Bi - 0.0001
Ag - 0.0005
Zr 0.01 0.04

HR55 - Detail

Specification for nickel-iron-chromium-molybdenum-aluminium-titanium heat-resisting alloy billets, bars, forgings and parts (Ni/Co 43.5, Cr 16.5, Mo 3.3, Al 1.2, Ti 1.2, Fe remainder)

Mechanical properties of grade HR55 BS 2HR 55 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
668 (≥) 187 (≥) 43 34 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 221

Physical properties of grade HR55 BS 2HR 55 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
412 (≥) 764 (≥) 11 42 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 342
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
865 651 759

Equivalent Grade

Equivalent Products