05X7H13ΓT Stainless Steels

05X7H13ΓT - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 05X7H13ΓT grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 0.60
Mn 0.80 1.20
P - 0.020
S - 0.020
Cr 6.00 7.50
Ni 12.50 14.00
Mo - 0.20
Nb 0.70 1.20
B 0.001 0.005
Ce 0.10 0.20

05X7H13ΓT - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 05X7H13ΓT

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
365 (≥) 163 (≥) 22 31 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 323

Physical properties of grade 05X7H13ΓT

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
214 (≥) 454 (≥) 34 21 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 424
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
863 223 414

Equivalent Grade

Equivalent Products

We can customize the production of 05X7H13ΓT grade, contact us for the best solution.