1.2316 Tool Die Steels to DIN 17350 (1980)

1.2316 - Specification & Application

  • DIN 17350 (1980) - Tool Steels; Technical Conditions of Delivery

Tool Steels; Technical Conditions of Delivery

Chemical composition(wt.%) of 1.2316 grade: to DIN 17350 (1980)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.33 0.43
Si - 1.00
Mn - 1.00
P - 0.030
S - 0.030
Cr 15.00 17.00
Mo 1.00 1.30
V - -
Ni - 1.00

1.2316 - Detail

Tool Steels; Technical Conditions of Delivery

Mechanical properties of grade 1.2316 DIN 17350 (1980)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
215 (≥) 177 (≥) 23 23 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 134

Physical properties of grade 1.2316 DIN 17350 (1980)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
573 (≥) 872 (≥) 34 11 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 311
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
181 581 182

Equivalent Grade

Equivalent Products

We can customize the production of 1.2316 grade, contact us for the best solution.