1.4001 Stainless Steels

1.4001 - Specification & Application

Armatures, building fittings, cutlery

Chemical composition(wt.%) of 1.4001 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.030
Cr 13.0 15.0

1.4001 - Detail

Stainless steels - Technical delivery conditions for drawn wire
Ferritic stainless steel

Mechanical properties of grade 1.4001

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
624 (≥) 319 (≥) 23 34 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 223

Physical properties of grade 1.4001

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
549 (≥) 552 (≥) 23 21 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 111
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
231 418 634

Equivalent Grade

Equivalent Products

We can customize the production of 1.4001 grade, contact us for the best solution.
sales@specificsteel.com