  • SEW 400 - Stainless steels for rolled and forged products

Stainless steels - Part 3: Technical dStainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposeselivery conditions for semi-finishe

Chemical composition(wt.%) of 1.4110 grade: to DIN EN 10088-1

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.60 0.75
Si - 0.70
Mn - 1.00
P - 0.040
S - 0.015
Cr 14.0 16.0
Mo 0.40 0.80

1.4110 - Detail

Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes

Mechanical properties of grade 1.4110 DIN EN 10088-1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
489 (≥) 145 (≥) 13 12 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 421

Physical properties of grade 1.4110 DIN EN 10088-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
139 (≥) 993 (≥) 14 22 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 414
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
625 316 645

Equivalent Grade

Equivalent Products

We can customize the production of 1.4110 grade, contact us for the best solution.