1.4111 Stainless Steels

1.4111 - Specification & Application

High alloyed CrMoV stainless steel

Chemical composition(wt.%) of 1.4111 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 1.05 1.15
Si - 1.00
Mn - 1.00
P - 0.045
S - 0.030
Cr 14.0 16.0
Mo 0.40 0.80
V 0.10 0.15

1.4111 - Detail

High alloyed CrMoV stainless steel

Mechanical properties of grade 1.4111

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
669 (≥) 496 (≥) 31 41 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 242

Physical properties of grade 1.4111

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
653 (≥) 317 (≥) 42 33 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 431
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
352 831 778

Equivalent Grade